e7018 - bajo contenido de hidrógeno / alta resistencia - electrodo / varilla de soldadura - 14 "x 1/8"

  • Marca:

    tgb

  • Código producto: B07CX7W85J
  • Disponibilidad: Traemos a pedido, tiempo de 15 a 25 dias.
  • $CLP 216.084

TÉRMINOS Y CONDICIONES

------------------------------------------

- El producto se trae a pedido, en un transcurso de 15 a 25 dias, si alguna restriccion de un ente gubernamental o de salud publica cambia o restringe vuelos, los pedidos pueden demorar mas tiempo.
- Precios pueden cambiar previo aviso. Depende de precio con proveedores o existencia.
- Fotos referenciales del producto, consulte no mas
- Despachamos a todo Chile con Starken.
- Productos importados de Estados Unidos, es probable que los productos electronicos trabajen en 110V y NO en 220V, podria usar un transformador, para mas informacion primero nos puedes preguntar todas las inquietudes que tengas.
-A low-hydrogen, all-position electrode for welding carbon steel, high-tensile steel, low alloy steel and free-machining steels - AWS/SFA 5.1 E7018 - AC/DC+ (Reverse Polarity)
-Quiet steady arc, low spatter, superb re-striking capabilities and high deposition efficiency all made possible by the special low-hydrogen iron powder coating and graphite tip
-Easily removable slag reveals a finely rippled bead appearance and an x-ray quality weld deposit with excellent charpy impact values at sub-zero temperatures (78 ft-lbs at -2-F)
-Typical applications include structural and fabrication steels such as I-beams, angles, plates, channels, cast steels, cold rolled steel, process piping steels and shipbuilding steels
-Select your Electrode Diameter and Package Quantity from the Options - Check Picture #3 for Welding Parameters.

Instructions: Use this electrode with DC+ (reverse polarity), however, an AC machine with sufficient open circuit voltage may be used. Clean the weld zone of all contaminants. Bevel thick sections to a 6- Vee and preheat at 300-50-F. Set amperage to the proper range as listed on the product recommended amperage chart. Maintain a short arc length and hold the electrode at a 1- angle into the direction of travel. Weaving technique is preferred, however, do not exceed 3 times the diameter of the electrode. Do not use the whipping technique as this will cause porosity in the weld deposit. Always allow high-carbon steels to cool slowly before removing the slag.